VE633 VE532

Silverhalide Emulsions / Chemistry.
Valery
Posts: 278
Joined: Fri Jan 09, 2015 12:42 pm
Location: Yaroslavl , Russia

VE633 VE532

Post by Valery »

The Dear Friends , colleagues.
Many have got from me films VE633 VE532.
Please write its opinion.
If there is questions and wish. :)
Valery.
Johnfp

VE633 VE532

Post by Johnfp »

Excellent. I was going to start a thread for discussion on the film myself as soon as I produced some holograms.
I hope to do some holograms with your film this weekend. I am very excited to try it.
Thanks again Valery.
Valery
Posts: 278
Joined: Fri Jan 09, 2015 12:42 pm
Location: Yaroslavl , Russia

VE633 VE532

Post by Valery »

It is Important.
If you work with film PET base 18 cm width of the roll of the edge of the film have a salients , this I have did therefor that film in roll less scetched, she will rest in edges.
But if jam this film between two glass, that film tightly to press impossible ( disturb the edges) their better cut or press the vacuum
Johnfp

VE633 VE532

Post by Johnfp »

Please check my understanding:

I have 12 cm VE633
Is it TAC or PET?

To get a GOLD reflection hologram H2
Use GP-2 dev, then fixer with no bleach.

To get a RED master H1 hologram
Pretreat? or Posttreat? with 6-20% sorbitol in ethanol?
Then Dev and bleach.

Also, do I cut the long edge for the VE633 film I have? I am not sure if it is PET or TAC.

Thank you,
JOhn
Johnfp

VE633 VE532

Post by Johnfp »

Dave, have you tried anything on this film yet?
Valery
Posts: 278
Joined: Fri Jan 09, 2015 12:42 pm
Location: Yaroslavl , Russia

VE633 VE532

Post by Valery »

Johnfp wrote:Please check my understanding:

I have 12 cm VE633
Is it TAC or PET?

To get a GOLD reflection hologram H2
Use GP-2 dev, then fixer with no bleach.

To get a RED master H1 hologram
Pretreat? or Posttreat? with 6-20% sorbitol in ethanol?
Then Dev and bleach.

Also, do I cut the long edge for the VE633 film I have? I am not sure if it is PET or TAC.

Thank you,
JOhn
I not litter what film you has, but PET in a complicated way to break, TAC to break simply.

I use GP-2 for H1 and H2. Without bleach.

6-20% sorbitol are used for reception red ( not gold(en)) reflection hologram.Posttreat.
Johnfp

VE633 VE532

Post by Johnfp »

Thank you!
holomaker
Posts: 772
Joined: Wed Jan 07, 2015 8:01 am

VE633 VE532

Post by holomaker »

Johnfp wrote:Dave, have you tried anything on this film yet?

hi John, ive only done a quick fog/saflight test (amber leds and kodak #13 filter work fine for the 532nm film), ive ordered chems to make some G2 developer, i did my tests using D-19/chrome bleach with less than optimum results (really wrong developer/bleach was used)............
Post Reply